Influence of Deposition Condition on Y2O3 Coatings Produced by Pulsed Electrophoretic Deposition

Y2O3 nanoparticle suspension aqueous solution was prepared using citric acid. Then, Y2O3 film was deposited using this solution with pulsed electrophoretic deposition (EPD). A dense Y2O3 film of 25.7 μm thickness was obtained with deposition conditions of 0.5 wt% Y2O3 concentration, bias voltage of...