Effect of TiB content on the properties of Al-TiB composites

In this study, titanium boride (TiB) was used to make Al-TiB composites. The contents of TiB added into Al matrix were 1 wt.%, 5 wt.% and 10 wt.%, respectively. The composites were pressed at a pressure of 382 MPa and sintered at 600°C for 4 hours. The microstructures and properties of d...

Full description

Bibliographic Details
Main Authors: Yang Shen, Guo Zuoxing, Xia Maosheng
Format: Article
Language:English
Published: International Institute for the Science of Sintering, Beograd 2018-01-01
Series:Science of Sintering
Subjects:
Online Access:http://www.doiserbia.nb.rs/img/doi/0350-820X/2018/0350-820X1802237Y.pdf
id doaj-3b3c3cd35ea543ae994230938c7d0f2c
record_format Article
spelling doaj-3b3c3cd35ea543ae994230938c7d0f2c2020-11-25T02:29:36ZengInternational Institute for the Science of Sintering, BeogradScience of Sintering0350-820X1820-74132018-01-0150223724410.2298/SOS1802237Y0350-820X1802237YEffect of TiB content on the properties of Al-TiB compositesYang Shen0Guo Zuoxing1Xia Maosheng2Jilin University, Ministry of Education, College of Materials Science and Engineering, The key Lab of Automobile Materials, Changchun, ChinaJilin University, Ministry of Education, College of Materials Science and Engineering, The key Lab of Automobile Materials, Changchun, ChinaJilin University, Ministry of Education, College of Materials Science and Engineering, The key Lab of Automobile Materials, Changchun, ChinaIn this study, titanium boride (TiB) was used to make Al-TiB composites. The contents of TiB added into Al matrix were 1 wt.%, 5 wt.% and 10 wt.%, respectively. The composites were pressed at a pressure of 382 MPa and sintered at 600°C for 4 hours. The microstructures and properties of density, hardness and wear were investigated. Experimental results indicated that, the composite with 5 wt.% TiB owned the highest relative density and hardness among the three parameters. In addition, TiB particles dramatically improved the wear resistance of the Al matrix and the more TiB content the better of the wear resistance. That is, the composite with 10 wt.% TiB owned the best wear resistance.http://www.doiserbia.nb.rs/img/doi/0350-820X/2018/0350-820X1802237Y.pdfTitanium boride (TiB)Al-TiB compositesdensityhardnesswear
collection DOAJ
language English
format Article
sources DOAJ
author Yang Shen
Guo Zuoxing
Xia Maosheng
spellingShingle Yang Shen
Guo Zuoxing
Xia Maosheng
Effect of TiB content on the properties of Al-TiB composites
Science of Sintering
Titanium boride (TiB)
Al-TiB composites
density
hardness
wear
author_facet Yang Shen
Guo Zuoxing
Xia Maosheng
author_sort Yang Shen
title Effect of TiB content on the properties of Al-TiB composites
title_short Effect of TiB content on the properties of Al-TiB composites
title_full Effect of TiB content on the properties of Al-TiB composites
title_fullStr Effect of TiB content on the properties of Al-TiB composites
title_full_unstemmed Effect of TiB content on the properties of Al-TiB composites
title_sort effect of tib content on the properties of al-tib composites
publisher International Institute for the Science of Sintering, Beograd
series Science of Sintering
issn 0350-820X
1820-7413
publishDate 2018-01-01
description In this study, titanium boride (TiB) was used to make Al-TiB composites. The contents of TiB added into Al matrix were 1 wt.%, 5 wt.% and 10 wt.%, respectively. The composites were pressed at a pressure of 382 MPa and sintered at 600°C for 4 hours. The microstructures and properties of density, hardness and wear were investigated. Experimental results indicated that, the composite with 5 wt.% TiB owned the highest relative density and hardness among the three parameters. In addition, TiB particles dramatically improved the wear resistance of the Al matrix and the more TiB content the better of the wear resistance. That is, the composite with 10 wt.% TiB owned the best wear resistance.
topic Titanium boride (TiB)
Al-TiB composites
density
hardness
wear
url http://www.doiserbia.nb.rs/img/doi/0350-820X/2018/0350-820X1802237Y.pdf
work_keys_str_mv AT yangshen effectoftibcontentonthepropertiesofaltibcomposites
AT guozuoxing effectoftibcontentonthepropertiesofaltibcomposites
AT xiamaosheng effectoftibcontentonthepropertiesofaltibcomposites
_version_ 1724832137548398592