Evaluation of surface roughness of the bracket slot before and after burning

Slot bracket base is one important element to enable sliding movement of the archwire. Bracket reconditioning by means of burning changes the surface roughness of slot bracket base. The heat above 450 °C shows microstructure changes of the slot surface. On this basis, the present study aims to evalu...