Elimination of Negative Effect of Fe in Secondary Alloys AlSi6Cu4 (En Ac 45 000, A 319) by Nickel
Artykuł opisuje wpływ dodatku niklu| do stopów wtórnych Al-Si-Cu na segregację faz zawierających żelazo, które jest jednym z najpowszechniej występujących zanieczyszczeń w tych stopach. Powszechnie wiadomo, iż nie jest możliwe usunięcie żelaza z kąpieli metalowej, natomiast można ograniczać negatyw...
Main Authors: | , , |
---|---|
Format: | Article |
Language: | English |
Published: |
Polish Academy of Sciences
2014-06-01
|
Series: | Archives of Metallurgy and Materials |
Subjects: | |
Online Access: | http://www.degruyter.com/view/j/amm.2014.59.issue-2/amm-2014-0118/amm-2014-0118.xml?format=INT |
id |
doaj-7f4e5f4c13e940e3baee908c6bca4300 |
---|---|
record_format |
Article |
spelling |
doaj-7f4e5f4c13e940e3baee908c6bca43002020-11-25T03:44:35ZengPolish Academy of SciencesArchives of Metallurgy and Materials2300-19092014-06-0159271772110.2478/amm-2014-0118amm-2014-0118Elimination of Negative Effect of Fe in Secondary Alloys AlSi6Cu4 (En Ac 45 000, A 319) by NickelBolibruchová D.0Macko J.1Brůna M.2UNIVERSITY OF ŽILINA, FACULTY OF MECHANICAL ENGINEERING, DEPARTMENT OF TECHNOLOGICAL ENGINEERING, SLOVAK REPUBLICUNIVERSITY OF ŽILINA, FACULTY OF MECHANICAL ENGINEERING, DEPARTMENT OF TECHNOLOGICAL ENGINEERING, SLOVAK REPUBLICUNIVERSITY OF ŽILINA, FACULTY OF MECHANICAL ENGINEERING, DEPARTMENT OF TECHNOLOGICAL ENGINEERING, SLOVAK REPUBLIC Artykuł opisuje wpływ dodatku niklu| do stopów wtórnych Al-Si-Cu na segregację faz zawierających żelazo, które jest jednym z najpowszechniej występujących zanieczyszczeń w tych stopach. Powszechnie wiadomo, iż nie jest możliwe usunięcie żelaza z kąpieli metalowej, natomiast można ograniczać negatywny jego wpływ poprzez związanie żelaza w fazach między- metalicznych mniej szkodliwych niż fazy β Fe, np. w następstwie dodatku innych pierwiastków. W badaniach do obróbki kąpieli zastosowano zaprawę AlNi20 z dokładnie określoną zawartością żelaza. Oddziały wanie niklu na skład i morfologię faz żelazowych określano na drodze analizy chemicznej (badania rozpuszczalności), analizy termicznej i oceny struktury. Na podstawie wyników badań stwierdzono, iż w badanych stopach nikiel nie wywiera wpływu na zmianę składu fazy (Z Fe, nie zmienia również kształtu jej wydzieleń do postaci bardziej korzystnej z punktu widzenia wpływu na właściwości.http://www.degruyter.com/view/j/amm.2014.59.issue-2/amm-2014-0118/amm-2014-0118.xml?format=INTIron based phasesthermal analysisiron based phases correctorsnickel |
collection |
DOAJ |
language |
English |
format |
Article |
sources |
DOAJ |
author |
Bolibruchová D. Macko J. Brůna M. |
spellingShingle |
Bolibruchová D. Macko J. Brůna M. Elimination of Negative Effect of Fe in Secondary Alloys AlSi6Cu4 (En Ac 45 000, A 319) by Nickel Archives of Metallurgy and Materials Iron based phases thermal analysis iron based phases correctors nickel |
author_facet |
Bolibruchová D. Macko J. Brůna M. |
author_sort |
Bolibruchová D. |
title |
Elimination of Negative Effect of Fe in Secondary Alloys AlSi6Cu4 (En Ac 45 000, A 319) by Nickel |
title_short |
Elimination of Negative Effect of Fe in Secondary Alloys AlSi6Cu4 (En Ac 45 000, A 319) by Nickel |
title_full |
Elimination of Negative Effect of Fe in Secondary Alloys AlSi6Cu4 (En Ac 45 000, A 319) by Nickel |
title_fullStr |
Elimination of Negative Effect of Fe in Secondary Alloys AlSi6Cu4 (En Ac 45 000, A 319) by Nickel |
title_full_unstemmed |
Elimination of Negative Effect of Fe in Secondary Alloys AlSi6Cu4 (En Ac 45 000, A 319) by Nickel |
title_sort |
elimination of negative effect of fe in secondary alloys alsi6cu4 (en ac 45 000, a 319) by nickel |
publisher |
Polish Academy of Sciences |
series |
Archives of Metallurgy and Materials |
issn |
2300-1909 |
publishDate |
2014-06-01 |
description |
Artykuł opisuje wpływ dodatku niklu| do stopów wtórnych Al-Si-Cu na segregację faz zawierających żelazo, które jest jednym z najpowszechniej występujących zanieczyszczeń w tych stopach. Powszechnie wiadomo, iż nie jest możliwe usunięcie żelaza z kąpieli metalowej, natomiast można ograniczać negatywny jego wpływ poprzez związanie żelaza w fazach między- metalicznych mniej szkodliwych niż fazy β Fe, np. w następstwie dodatku innych pierwiastków. W badaniach do obróbki kąpieli zastosowano zaprawę AlNi20 z dokładnie określoną zawartością żelaza. Oddziały wanie niklu na skład i morfologię faz żelazowych określano na drodze analizy chemicznej (badania rozpuszczalności), analizy termicznej i oceny struktury. Na podstawie wyników badań stwierdzono, iż w badanych stopach nikiel nie wywiera wpływu na zmianę składu fazy (Z Fe, nie zmienia również kształtu jej wydzieleń do postaci bardziej korzystnej z punktu widzenia wpływu na właściwości. |
topic |
Iron based phases thermal analysis iron based phases correctors nickel |
url |
http://www.degruyter.com/view/j/amm.2014.59.issue-2/amm-2014-0118/amm-2014-0118.xml?format=INT |
work_keys_str_mv |
AT bolibruchovad eliminationofnegativeeffectoffeinsecondaryalloysalsi6cu4enac45000a319bynickel AT mackoj eliminationofnegativeeffectoffeinsecondaryalloysalsi6cu4enac45000a319bynickel AT brunam eliminationofnegativeeffectoffeinsecondaryalloysalsi6cu4enac45000a319bynickel |
_version_ |
1724513876423213056 |