碩士 === 國立中央大學 === 機械工程學系 === 101 === A set of 7075-T73 alloy samples was prepared for running anodization in a 15wt% sulfuric acid solution to coat 10-12 micron in thickness of anodic aluminum oxide (AAO) film and then sealed in hot water. The samples with/without AAO film were removed for carrying...