Effect of Center Segregation of Hot-Rolled Rod on Mechanical Properties of Oil-Quenched and Tempered Spring Steel 55SiCrA
The production flowsheet of oil-quenched at 890 ℃ for 300 s and tempered at 530℃ for 1200 s Φ22 mm rod of spring steel 55SiCrA (/% : 0.55C, 1.45Si, 0.67Mn, 0.010P, 0.005S, 0.68Cr) is hot metal desulphurization- 80 t top and bottom combined blowing converter- LF- RH- 280 mm x 325 mm bloom casting-Φ22...