Synthesis of Pure Nano semiconductor Oxide ZnO with Different AgNO3 Concentrations

Zinc oxide nanoparticles sample is prepared by the precipitation method. This method involves using zinc nitrate and urea in aqueous solution, then (AgNO3) Solution with different concentrations is added. The obtained precipitated compound is structurally characterized by X-ray diffraction (XRD), Sc...

詳細記述

書誌詳細
出版年:مجلة بغداد للعلوم
第一著者: Baghdad Science Journal
フォーマット: 論文
言語:英語
出版事項: University of Baghdad, College of Science for Women 2017-06-01
主題:
オンライン・アクセス:http://bsj.uobaghdad.edu.iq/index.php/BSJ/article/view/2375
その他の書誌記述
要約:Zinc oxide nanoparticles sample is prepared by the precipitation method. This method involves using zinc nitrate and urea in aqueous solution, then (AgNO3) Solution with different concentrations is added. The obtained precipitated compound is structurally characterized by X-ray diffraction (XRD), Scanning electron microscopy (SEM), Atomic force microscopy (AFM) and Fourier transform infrared spectroscopy (FTIR). The average particle size of nanoparticles is around 28nm in pure, the average particle size reaches 26nm with adding AgNO3 (0.05g in100ml =0.002 M) (0.1g in100ml=0.0058M), AgNO3 (0.2g in 100ml=0.01M) was 25nm. The FTIR result shows the existence of -CO, -CO2, -OH, and -NO2- groups in sample and oxides (ZnO, Ag2O).and used an atomic force microscope and microscope scanning electron to model the record.
ISSN:2078-8665
2411-7986