On the effect of temperature on the threshold stress intensity factor of delayed hydride cracking in light water reactor fuel cladding

Delayed hydride cracking (DHC) was first observed in pressure tubes in Canadian CANDU reactors. In light water reactors, DHC was not observed until the late 1990s in high-burnup boiling water reactor (BWR) fuel cladding. In recent years, the focus on DHC has resurfaced in light of the increased inte...