Practice of Pilot Production on Φ350 mm Cast Round Bloom of Steel 4130 by 50 t EAF-LF (VD)-CC Flow Sheet

With using 50 t EAF-LF(VD)-CC-slow cooling pross, controlling EAF end [C] 0.12%-0.25% and end [P]≤ 0.015%, pre-deoxidizing and alloying in tapping, using CaO-Al<sub>2</sub>O<sub>3</sub>free fluorine pre-melting refining slag, and integrate casting control technology including...

Full description

Bibliographic Details
Published in:Teshugang
Main Author: Li Faxing
Format: Article
Language:Chinese
Published: Editorial Office of Special Steel 2013-09-01
Subjects:
Online Access:http://www.specialsteeljournal.com/thesisDetails?columnId=129789991&Fpath=home&index=0