Optimization of 180 t LF Deep Desulphurization Refining Process for Pipeline Steel X70

The production flow sheet for pipeline steel X70 is KR metal pre-desulphuration-180 t BOF-LF-RH-slab CC process. With optimization of refining slag ingredient and slagging operation, and based on effect of bottom gas blowing rate (400-700 L/min) on end [S] , the LF deep desulphurization process has...