Effect of LF Soft Bubbling Time on Inclusions in Tire Cord Steel LX82 A

For the control of cord steel inclusion, long time soft bubbling treatment is usually chosen to improve the cleanliness of molten steel, but it will lead to the increased erosion of magnesia-carbon bricks. Through the industrial production test, the effects of soft blowing time after LF refining on...