Hydrothermal synthesis of bioactive calcium silicate glass

This work presents the synthesis of bioactive glass 60SiO2-40CaO (wt.%) by the hydrothermal method without using acid catalysts in a shortened synthesis time. The precursors Si(OC2H5)4 (TEOS), Ca(NO3)2.4H2O were introduced in a hydrothermal system, and heated at 150 oC for 24 hours. The resulting ge...