Indentation Behavior Assessment of As-Built, Solution, and Artificial Aged Heat-Treated Selective Laser Melting Specimens of AlSi10Mg
This study was conducted to determine the indentation behavior of thin AlSi10Mg specimens manufactured using Selective Laser Melting (SLM) in the as-built condition along with two post-treatments, namely solution heat treatment and artificial aging. Four different thicknesses of 1.0 mm, 1.5 mm, 2 mm...