Controlled Rolling and Cooling Process Optimization of Non-annealed 12Cr1MoV Wire Rod Products for Boiler Flat Steel

In order to develop non-spheroidizing annealing 12Cr1MoV hot rolled wire rod , based on deformation induced phase transition mechanism, the finishing rolling temperature of 830 ℃ and laying temperature of 800 ℃ were adopted. By inhibiting deformation austenite grain recovery and recrystallization pr...