Crystallization of CuZrAgAl Bulk Metallic Glass at Various Temperatures and Pressures

The Cu₄₃Zr₄₃Ag₇Al₇ alloy was obtained in an amorphous form through inert gas spray forming, followed by separation using a tower cyclone gas separator. The resulting spherical particles were about 11 μm in size. The consolidation of the powder was carried out using two distinct methods. First, Spark...