Continuous cooling transformation diagrams of HSLA steel for seamless tubes production

The CCT and two DCCT diagrams were constructed for the HSLA steel containing Cr, V, Nb, and N microadditions, taking into account industrial processing parameters of this material in a seamless tubes rolling mill. The typical finish hot rolling temperature of 1173 K was used for the construction of...