Micro/Nano Indentation Testing of Spark Plasma Sintered Al<sub>2</sub>O<sub>3</sub> + ZrO<sub>2</sub> + cBN Ceramics
Al<sub>2</sub>O<sub>3</sub> + 30 vol% ZrO<sub>2</sub> matrix composites with 20 and 30 vol% cBN have been prepared with the optimized processing route, using spark plasma sintering (SPS) at temperatures of 1400 °C and 1250 °C. The influence of cBN addition on the...