Wear performance analysis and characterization of HVOF deposited Ni–20Cr2O3, Ni–30Al2O3, and Al2O3–13TiO2 coatings
The present study was aimed to analyze a slurry erosion failure of SS316L steel coated with high-velocity oxygen-fuel coatings using Ni–20Cr2O3, Ni–30Al2O3, and Al2O3–13TiO2. Slurry erosion experiments were performed using a pot erosion tester for the time duration of 90–180 min at different velocit...