The influence of the heat treatment on delta ferrite transformation in austenitic stainless steel welds

Shielded metal arc (SMAW) welded specimens using austenitic consumable materials with different amount of delta-ferrite are annealed in range 650-750 °C through 2-10 hours. Factorial plan 3<sup>3</sup> with influenced factors regression analyze of measured delta-ferrite values is used. T...