MEMBRAN POLIURETAN DARI MINYAK BIJI KARET (RUBBER SEED OIL) DENGAN HEKSAMETILEN-1,6-DIISOSIANAT: SINTESIS
Polyurethane membrane made from Rubber Seed Oil has been produced within this research. Rubber seed oil has the hydroxyl number of 40,33 mg/g and the iodine number of 154,05 g/g which can be used as resource clusters; -OH, in order to make polyurethane. Rubber seed oil can react with hexamethylen...
Main Authors: | , , |
---|---|
Format: | Article |
Language: | English |
Published: |
Universitas Syiah Kuala
2016-03-01
|
Series: | Jurnal Natural |
Online Access: | http://jurnal.unsyiah.ac.id/natural/article/view/4705 |
Summary: | Polyurethane membrane made from Rubber Seed Oil has been produced within this research. Rubber seed oil has the hydroxyl number of 40,33 mg/g and the iodine number of 154,05 g/g which can be used as resource clusters; -OH, in order to make polyurethane. Rubber seed oil can react with hexamethylene-1.6-diisocyanate (HDMI) as another resource cluster, which is -NCO. The production of polyurethane membrane is done by variating the composition of rubber seed oil and HDMI, with the variations of 5:1; 5:3; 5:4; 5:5 dan 5:7 (v/w) and the polymrization temperature of 90-100°C and the curring temperature of 165-170°C. The optimal polyurethane membrane is produced on the composition of 5:4 v/w which is homogenous, dry, quite elastic and is yellowish brown in colour. The IR results showed that there were urethan bonds formed (N-H on ν = 3300-3400 cm-1) and the TGA results from polyurethane membrane showed that there were two decompositions on 394,5oC dan 458,6oC. |
---|---|
ISSN: | 1411-8513 2541-4062 |