Fabrication Of Porous Ti By Thermal Decomposition And Sintering Of PMMA/TiH2 Powder Compact
Porous Ti with controlled pore structure was fabricated by thermal decomposition and sintering process using TiH2 powders and Polymethylmethacrylates (PMMA) beads as pore forming agent. The beads sizes of 8 and 50 μm were used as a template for fabricating the porous Ti. The TiH2 powder compacts wit...
Main Authors: | Jeon K.Ch., Kim Y.D., Suk M.-J., Oh S.-T. |
---|---|
Format: | Article |
Language: | English |
Published: |
Polish Academy of Sciences
2015-06-01
|
Series: | Archives of Metallurgy and Materials |
Subjects: | |
Online Access: | http://www.degruyter.com/view/j/amm.2015.60.issue-2/amm-2015-0134/amm-2015-0134.xml?format=INT |
Similar Items
-
Microstructural characterization and interactions in Ti- and TiH2-hydroxyapatite vacuum sintered composites
by: Marcelo Teresa Maria, et al.
Published: (2006-01-01) -
The Effects of Sintering Temperature and Addition of TiH<sub>2</sub> on the Sintering Process of Cu
by: Huali Hao, et al.
Published: (2019-08-01) -
Investigation on the Reaction Energy, Dynamic Mechanical Behaviors, and Impact-Induced Reaction Characteristics of PTFE/Al with Different TiH2 Percentages
by: Zhongshen Yu, et al.
Published: (2018-10-01) -
Effect of Sintering Factors on Properties of Al-Rich PTFE/Al/TiH<sub>2</sub> Active Materials
by: Yilei Wang, et al.
Published: (2021-05-01) -
Mechanical properties of TiO2-filled CNT/PMMA composites
by: He Runqin, et al.
Published: (2017-01-01)