Alloy degradation under oxidizing-sulfidizing conditions at elevated temperatures
Exposure of high-temperature alloys to a low-P O2 oxidizing-sulfidizing environment above about 550 °C is often characterized by an initial period of protective oxidation followed by more rapid corrosion. This paper will provide a brief overview of alloy corrosion in oxidizing-sulfidizing atmosphere...
Main Author: | Brian Gleeson |
---|---|
Format: | Article |
Language: | English |
Published: |
Associação Brasileira de Metalurgia e Materiais (ABM); Associação Brasileira de Cerâmica (ABC); Associação Brasileira de Polímeros (ABPol)
2004-03-01
|
Series: | Materials Research |
Subjects: | |
Online Access: | http://www.scielo.br/scielo.php?script=sci_arttext&pid=S1516-14392004000100010 |
Similar Items
-
High Temperature Oxidation Behavior of Fe-Cr Steel in Air at 1000-1200 K
by: T. Sudiro, et al.
Published: (2018-04-01) -
High temperature oxidation behavior of type 444 stainless steel in synthetic automotive exhaust gas
by: Jianming Zhan, et al.
Published: (2021-05-01) -
Dislocation Breakaway Damping in AA7050 Alloy
by: Andrea Di Schino, et al.
Published: (2020-12-01) -
Brownian coagulation of aerosols in transition regime
by: Chen Zhong-Li
Published: (2012-01-01) -
Enhanced Photocatalytic Degradation of Ternary Dyes by Copper Sulfide Nanoparticles
by: Peter A. Ajibade, et al.
Published: (2021-08-01)