Compressive Properties of A2024 Alloy Foam Fabricated through a Melt Route and a Semi-Solid Route
A2024 alloy foams were fabricated by two methods. In the first method, the melt was thickened by Mg, which acts as an alloying element (melt route). In the second method, the melt was thickened by using primary crystals at a semi-solid temperature with a solid fraction of 20% (semi-solid route). A20...
Main Authors: | Takashi Kuwahara, Taro Osaka, Mizuki Saito, Shinsuke Suzuki |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2019-01-01
|
Series: | Metals |
Subjects: | |
Online Access: | https://www.mdpi.com/2075-4701/9/2/153 |
Similar Items
-
Effect of Primary Crystals on Pore Morphology during Semi-Solid Foaming of A2024 Alloys
by: Takashi Kuwahara, et al.
Published: (2019-01-01) -
Percolation of Primary Crystals in Cell Walls of Aluminum Alloy Foam via Semi-Solid Route
by: Satomi Takamatsu, et al.
Published: (2020-06-01) -
Stabilization Mechanism of Semi-Solid Film Simulating the Cell Wall during Fabrication of Aluminum Foam
by: Takashi Kuwahara, et al.
Published: (2020-03-01) -
Permeability of Aluminium Foams Produced by Replication Casting
by: Maxim L. Cherny, et al.
Published: (2012-12-01) -
Damping properties of open pore aluminum foams produced by vacuum casting and NaCl dissolution process
by: L. Dahil, et al.
Published: (2013-10-01)