Catalytic Decomposition of HO over Manganese Oxides Supported on an Active Alumina
A series of manganese oxides loaded on to an active alumina support was prepared by impregnation methods and the resulting samples preheated in air at 400°C, 650°C or 900°C for 6 h. The amount of manganese, expressed as Mn 2 O 3 , was varied between 3.7 wt% and 55.3 wt%. The kinetics of the decompos...
Main Authors: | Nasr-Allah M. Deraz, M.A. El-Sayed, A. Abd. El-Aal |
---|---|
Format: | Article |
Language: | English |
Published: |
Hindawi - SAGE Publishing
2001-09-01
|
Series: | Adsorption Science & Technology |
Online Access: | https://doi.org/10.1260/0263617011494385 |
Similar Items
-
Catalytic Decomposition of HO on CoO Doped with AgO or ZnO
by: Gamil A. El-Shobaky, et al.
Published: (2000-10-01) -
Catalytic Decomposition of HO over Pure and LiO-Doped CoO Solids
by: Gamil A. El-Shobaky, et al.
Published: (1998-10-01) -
The Effect of Calcium Doping on the Surface and Catalytic Properties of Cobaltic Oxide Catalysts
by: Nasr-Allah M. Deraz
Published: (2003-04-01) -
Hydrogen production via catalytic methane decomposition over alumina supported iron catalyst
by: Anis H. Fakeeha, et al.
Published: (2018-03-01) -
Catalytic oxidative desulfurization of diesel fuel utilizing alumina supported cobalt manganese oxides
by: Fathi Jasni, M. Jasmin
Published: (2012)