BEBERAPA SIFAT FISIS DAN KIMIA BRIKET ARANG DARI LIMBAH ARANG AKTIF

The result of  a study on briqueting charcoal from activated charcoal residue,  prepared  by using the hydraulic  press process is presented  in this paper. The residue :  was subjected to two different treatments, namely unwashed  and  washed with  water.  Following   the  treatment, each residue ...

Full description

Bibliographic Details
Main Authors: Gustan Pari, Djeni Hendra, Hartoyo Hartoyo
Format: Article
Language:Indonesian
Published: Forest Product Research and Development Center 2017-08-01
Series:Jurnal Penelitian Hasil Hutan (Journal of Forest Products Research)
Online Access:http://ejournal.forda-mof.org/ejournal-litbang/index.php/JPHH/article/view/3444
id doaj-94be55e1f9924f3eb14003abdd750574
record_format Article
spelling doaj-94be55e1f9924f3eb14003abdd7505742020-11-25T01:06:09ZindForest Product Research and Development CenterJurnal Penelitian Hasil Hutan (Journal of Forest Products Research)0216-43292442-89572017-08-0172616710.20886/jphh.1990.7.2.61 - 672439BEBERAPA SIFAT FISIS DAN KIMIA BRIKET ARANG DARI LIMBAH ARANG AKTIFGustan Pari0Djeni Hendra1Hartoyo Hartoyo2Pusat Penelitian dan Pengembangan Hasil HutanPusat Penelitian dan Pengembangan Hasil HutanPusat Penelitian dan Pengembangan Hasil HutanThe result of  a study on briqueting charcoal from activated charcoal residue,  prepared  by using the hydraulic  press process is presented  in this paper. The residue :  was subjected to two different treatments, namely unwashed  and  washed with  water.  Following   the  treatment, each residue  material  was mixed  with  starch adhesive, using four different concentrations:  0 percent, 1 percent, 2 percent  and 3 percent,  consecutively. The  respons  evaluated from the  briquetted charcoal are the  moisture content, ash content, volatile matter, fixed carbon, density, crushing strength and calorific value. The result shows  that  moisture  content ranges from  3,36 - 5,56 percent, ash content  from  8,06  - 12,78 percent, volatile matter from  23,56 - 41,28 percent, fixed carbon from  45,9 - 68,38  percent, density from 0,6471-0,7985 gr/cm, crushing strength from 0,79 - 6,33 kg/cm and  the  calorific values ranged from 5243,25  -  6378,84  cal/gr.http://ejournal.forda-mof.org/ejournal-litbang/index.php/JPHH/article/view/3444
collection DOAJ
language Indonesian
format Article
sources DOAJ
author Gustan Pari
Djeni Hendra
Hartoyo Hartoyo
spellingShingle Gustan Pari
Djeni Hendra
Hartoyo Hartoyo
BEBERAPA SIFAT FISIS DAN KIMIA BRIKET ARANG DARI LIMBAH ARANG AKTIF
Jurnal Penelitian Hasil Hutan (Journal of Forest Products Research)
author_facet Gustan Pari
Djeni Hendra
Hartoyo Hartoyo
author_sort Gustan Pari
title BEBERAPA SIFAT FISIS DAN KIMIA BRIKET ARANG DARI LIMBAH ARANG AKTIF
title_short BEBERAPA SIFAT FISIS DAN KIMIA BRIKET ARANG DARI LIMBAH ARANG AKTIF
title_full BEBERAPA SIFAT FISIS DAN KIMIA BRIKET ARANG DARI LIMBAH ARANG AKTIF
title_fullStr BEBERAPA SIFAT FISIS DAN KIMIA BRIKET ARANG DARI LIMBAH ARANG AKTIF
title_full_unstemmed BEBERAPA SIFAT FISIS DAN KIMIA BRIKET ARANG DARI LIMBAH ARANG AKTIF
title_sort beberapa sifat fisis dan kimia briket arang dari limbah arang aktif
publisher Forest Product Research and Development Center
series Jurnal Penelitian Hasil Hutan (Journal of Forest Products Research)
issn 0216-4329
2442-8957
publishDate 2017-08-01
description The result of  a study on briqueting charcoal from activated charcoal residue,  prepared  by using the hydraulic  press process is presented  in this paper. The residue :  was subjected to two different treatments, namely unwashed  and  washed with  water.  Following   the  treatment, each residue  material  was mixed  with  starch adhesive, using four different concentrations:  0 percent, 1 percent, 2 percent  and 3 percent,  consecutively. The  respons  evaluated from the  briquetted charcoal are the  moisture content, ash content, volatile matter, fixed carbon, density, crushing strength and calorific value. The result shows  that  moisture  content ranges from  3,36 - 5,56 percent, ash content  from  8,06  - 12,78 percent, volatile matter from  23,56 - 41,28 percent, fixed carbon from  45,9 - 68,38  percent, density from 0,6471-0,7985 gr/cm, crushing strength from 0,79 - 6,33 kg/cm and  the  calorific values ranged from 5243,25  -  6378,84  cal/gr.
url http://ejournal.forda-mof.org/ejournal-litbang/index.php/JPHH/article/view/3444
work_keys_str_mv AT gustanpari beberapasifatfisisdankimiabriketarangdarilimbaharangaktif
AT djenihendra beberapasifatfisisdankimiabriketarangdarilimbaharangaktif
AT hartoyohartoyo beberapasifatfisisdankimiabriketarangdarilimbaharangaktif
_version_ 1725191106635759616