Oxalate-assisted solvothermal synthesis of octahedral LiMn1.5Ni0.5O4 particles for lithium-ion batteries

Submicron octahedral LiMn1.5Ni0.5O4 particles were easily prepared by solvothermal synthesis method. The effects of synthesis conditions including precursors' concentration (0.09 and 0.18 M), calcination temperature (700 and 800 °C), and calcination time (2 and 8 h) were studied by modern chara...