Enhancement in (BH)max of PLD-made isotropic Nd-Fe-B thick film magnets deposited on Si substrates
Increase in Nd contents of a PLD-made isotropic Nd-Fe-B thick-film magnet enabled us to enhance the thickness of the film magnet deposited on a Si substrate because the linear expansion coefficient of Nd is an intermediate value between Nd2Fe14B and Si. The large amount of Nd, however, degraded the...
Main Authors: | M. Nakano, Y. Chikuba, D. Shimizu, A. Yamashita, T. Yanai, H. Fukunaga |
---|---|
Format: | Article |
Language: | English |
Published: |
AIP Publishing LLC
2017-05-01
|
Series: | AIP Advances |
Online Access: | http://dx.doi.org/10.1063/1.4979688 |
Similar Items
-
Preparation of Nd-Fe-B/α-Fe nano-composite thick-film magnets on various substrates using PLD with high laser energy density above 10 J/cm2
by: M. Nakano, et al.
Published: (2018-05-01) -
PLD-fabricated Pr-Fe-B thick film magnets applied to small motors
by: M. Nakano, et al.
Published: (2020-01-01) -
Magnetic properties of Pr-Fe-B thick-film magnets deposited on Si substrates with glass buffer layer
by: M. Nakano, et al.
Published: (2018-05-01) -
Study of sintered Nd-Fe-B magnet with high performance of Hcj (kOe) + (BH)max (MGOe) > 75
by: Bo-Ping Hu, et al.
Published: (2013-04-01) -
Isotropic nanocrystalline (Nd,Pr)(Fe,Co)B permanent magnets
by: Bollero Real, Alberto
Published: (2003)