Hot Corrosion of Co-based Alloys with 25%NaCl+75%Na2SO4 Coating at 1173 K
Hot corrosion behavior of pure Co, Co-10Cr and Co-10Cr-5Al alloys in the presence of a salt coat of Na2SO4+NaCl in air at 1173 K was studied. The results indicated that among the three samples, the mass gain of Co-10Cr-5Al alloy is the smallest, while that of Co-10Cr is biggest. The corrosion produc...
Main Authors: | Fu Guangyan, Guo Xingxing, Liu Qun, Zhao Xin, Su Yong |
---|---|
Format: | Article |
Language: | English |
Published: |
De Gruyter
2013-06-01
|
Series: | High Temperature Materials and Processes |
Subjects: | |
Online Access: | https://doi.org/10.1515/htmp-2012-0134 |
Similar Items
-
Hot Corrosion Behavior of a Novel Co-base Superalloy in Molten NaCl at 900℃
by: ZHANG Ying, et al.
Published: (2018-08-01) -
High Temperature Corrosion of Aluminized AISI 4130 Steel with the Different Composition of NaCl/Na2SO4 Deposits
by: Mohammad Badaruddin, et al.
Published: (2015-08-01) -
Pengaruh Pemberian Garam (NaCl) terhadap Kerusakan Telur Argulus Japonicus <br><i>[Effect of Salt (NaCl) Against Damage of Argulus japonicus Egg]<i>
by: Kismiyati Kismiyati, et al.
Published: (2011-04-01) -
Increasing NaCl Concentration by Using Precipitation and Filtration Process at Optimum Temperature
by: Maysoon Anwar Abdulla
Published: (2017-02-01) -
Increasing NaCl Concentration by Using Precipitation and Filtration Process at Optimum Temperature
by: Maysoon Anwar Abdulla
Published: (2017-02-01)