Effect of pH on Stress Corrosion Cracking of 6082 Al Alloy
In this work, the effect of pH (3, 7 and 10) on the stress corrosion cracking behavior of 6082 aluminum alloy, in a 0.3 M sodium chloride (NaCl) aqueous based solution was investigated. The stress corrosion cracking behavior was studied with slow strain rate testing, whereas failure analysis of the...
Main Authors: | C. N. Panagopoulos, Emmanuel Georgiou, K. I. Giannakopoulos, P. G. Orfanos |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2018-07-01
|
Series: | Metals |
Subjects: | |
Online Access: | http://www.mdpi.com/2075-4701/8/8/578 |
Similar Items
-
Dynamic Recrystallization Behavior and Processing Map of the 6082 Aluminum Alloy
by: Dao-chun Hu, et al.
Published: (2020-02-01) -
The Corrosion Inhibition of AA6082 Aluminium Alloy by Certain Azoles in Chloride Solution: Electrochemistry and Surface Analysis
by: Klodian Xhanari, et al.
Published: (2019-06-01) -
Investigation on Compressive Formability and Microstructure Evolution of 6082-T6 Aluminum Alloy
by: Zhouli Xu, et al.
Published: (2020-04-01) -
Crystal Orientation Evolution During Friction Stir Welding of 6082 Aluminum Alloys
by: ZHANG Liang-liang, et al.
Published: (2018-10-01) -
Experimental Studies on Corrosion Behavior of Ceramic Surface Coating using Different Deposition Techniques on 6082-T6 Aluminum Alloy
by: Ali Algahtani, et al.
Published: (2018-11-01)