Comparative evaluation of effect of laser on shear bond strength of ceramic bonded with two base metal alloys: An in-vitro study
The most common clinical failure in metal ceramic restoration is at the ceramo-metal interface. For the clinical longevity, metal-ceramic prostheses must have satisfactory bond strength between metal and ceramic. Aim and Objective: The aim of this study is to evaluate the effect of Laser etching on...
Main Authors: | K Deepak, S C Ahila, B Muthukumar, M Vasanthkumar |
---|---|
Format: | Article |
Language: | English |
Published: |
Wolters Kluwer Medknow Publications
2013-01-01
|
Series: | Indian Journal of Dental Research |
Subjects: | |
Online Access: | http://www.ijdr.in/article.asp?issn=0970-9290;year=2013;volume=24;issue=5;spage=610;epage=615;aulast=Deepak |
Similar Items
-
Evaluation of bond strength between grooved titanium alloy implant abutments and provisional veneering materials after surface treatment of the abutments: An in vitro study
by: Gowtham Venkat, et al.
Published: (2017-01-01) -
Shear bond strength of metal and ceramic brackets using conventional acid etch/primer and self-etch primer
by: Chandrika Katti, et al.
Published: (2019-01-01) -
In Vitro Evaluation of Shear Bond Strength of Self Etching Primers to Dentin
by: Reena Vora
Published: (2012-01-01) -
In Vitro Study of Shear Bond Strength in Direct and Indirect Bonding with Three Types of Adhesive Systems
by: Angelica Iglesias, et al.
Published: (2020-06-01) -
Shear bond strength of orthodontic buccal tubes to porcelain
by: Kathiravan Purmal, et al.
Published: (2013-01-01)