Mechanical and durability properties of GFRP bars exposed to aggressive solution environments
Two categories of GFRP specimens, in nominal diameters of 11.2 mm and 15.6 mm respectively, made of E-glass fibers and a vinylester resin were immersed in alkaline solution, saline solution and tap water solution at room temperature. The mechanical and durability properties of tested GFRP bar specim...
Main Authors: | Lu Chunhua, Yang Yuting, He Liyuan |
---|---|
Format: | Article |
Language: | English |
Published: |
De Gruyter
2021-01-01
|
Series: | Science and Engineering of Composite Materials |
Subjects: | |
Online Access: | https://doi.org/10.1515/secm-2021-0002 |
Similar Items
-
Prediction of the Long-Term Performance and Durability of GFRP Bars under the Combined Effect of a Sustained Load and Severe Environments
by: Jianwei Tu, et al.
Published: (2020-05-01) -
Strength Degradation of Gfrp Bars
by: Bhise, Vikrant Sudhakar
Published: (2014) -
Behavior of reinforced concrete beams reinforced with GFRP bars
by: D. H. Tavares, et al. -
Tensile Strength and Degradation of GFRP Bars under Combined Effects of Mechanical Load and Alkaline Solution
by: Qingping Jin, et al.
Published: (2020-08-01) -
Durability Prediction of GFRP Rebar Based on Elastic Modulus Degradation
by: Jianwei Tu, et al.
Published: (2019-10-01)