Tensile properties and fracture characteristics of spray cast alloy IC6 (Ni-7.8Al-14Mo-0.05B)
Tensile testing results of spray cast Ni3Al-based superalloy indicated that the yield strength and tensile strength increase with the increasing of temperature and reached maximum at around 760℃, then decrease with the increasing of temperature. After high temperature isostatic pressing (HIP), yield...