Effect of Wast Glass and Steel Slag on the Engineering Properties of HPC

碩士 === 國立雲林科技大學 === 營建工程系碩士班 === 90 === The objective of this study is to investigate the workability, compressive strength, and durability of concrete using waste glass and steel slag to replace the fine aggregate. The waste glasses and steel slag used for concrete include powders with 3000 and 500...

Full description

Bibliographic Details
Main Authors: Wang, Hung-Tsung, 王鴻宗
Other Authors: Su, Nan
Format: Others
Language:zh-TW
Published: 2002
Online Access:http://ndltd.ncl.edu.tw/handle/50950093394419328724
id ndltd-TW-090YUNTE582014
record_format oai_dc
spelling ndltd-TW-090YUNTE5820142016-06-24T04:15:30Z http://ndltd.ncl.edu.tw/handle/50950093394419328724 Effect of Wast Glass and Steel Slag on the Engineering Properties of HPC 玻璃、煉鋼爐碴應用於高性能混凝土之工程性質研究 Wang, Hung-Tsung 王鴻宗 碩士 國立雲林科技大學 營建工程系碩士班 90 The objective of this study is to investigate the workability, compressive strength, and durability of concrete using waste glass and steel slag to replace the fine aggregate. The waste glasses and steel slag used for concrete include powders with 3000 and 5000 Blaine to replace 5%, 10% and 15% of fine aggregate in concrete mixture. Test results show that 3000 Blaine of waste glass can improve the workability of fresh concrete, but the 5000 Blaine of waste glass and steel slag can’t. The compressive strength of concrete is higher than the control. The durability of concrete (including the thaw-freeze resistance, the chloride permeability, the anti-carbonation properties) can be improved by adding waste glass and steel slag in concrete, but the abrasion properties is lower than control. The drying shrinkage of mortar with waste glass and steel slag is higher the control. The microstructure analysis shows that the pozzolanic reaction occurs in cement paste with waste glass and steel slag powder. Su, Nan 蘇南 2002 學位論文 ; thesis 165 zh-TW
collection NDLTD
language zh-TW
format Others
sources NDLTD
description 碩士 === 國立雲林科技大學 === 營建工程系碩士班 === 90 === The objective of this study is to investigate the workability, compressive strength, and durability of concrete using waste glass and steel slag to replace the fine aggregate. The waste glasses and steel slag used for concrete include powders with 3000 and 5000 Blaine to replace 5%, 10% and 15% of fine aggregate in concrete mixture. Test results show that 3000 Blaine of waste glass can improve the workability of fresh concrete, but the 5000 Blaine of waste glass and steel slag can’t. The compressive strength of concrete is higher than the control. The durability of concrete (including the thaw-freeze resistance, the chloride permeability, the anti-carbonation properties) can be improved by adding waste glass and steel slag in concrete, but the abrasion properties is lower than control. The drying shrinkage of mortar with waste glass and steel slag is higher the control. The microstructure analysis shows that the pozzolanic reaction occurs in cement paste with waste glass and steel slag powder.
author2 Su, Nan
author_facet Su, Nan
Wang, Hung-Tsung
王鴻宗
author Wang, Hung-Tsung
王鴻宗
spellingShingle Wang, Hung-Tsung
王鴻宗
Effect of Wast Glass and Steel Slag on the Engineering Properties of HPC
author_sort Wang, Hung-Tsung
title Effect of Wast Glass and Steel Slag on the Engineering Properties of HPC
title_short Effect of Wast Glass and Steel Slag on the Engineering Properties of HPC
title_full Effect of Wast Glass and Steel Slag on the Engineering Properties of HPC
title_fullStr Effect of Wast Glass and Steel Slag on the Engineering Properties of HPC
title_full_unstemmed Effect of Wast Glass and Steel Slag on the Engineering Properties of HPC
title_sort effect of wast glass and steel slag on the engineering properties of hpc
publishDate 2002
url http://ndltd.ncl.edu.tw/handle/50950093394419328724
work_keys_str_mv AT wanghungtsung effectofwastglassandsteelslagontheengineeringpropertiesofhpc
AT wánghóngzōng effectofwastglassandsteelslagontheengineeringpropertiesofhpc
AT wanghungtsung bōlíliàngānglúcháyīngyòngyúgāoxìngnénghùnníngtǔzhīgōngchéngxìngzhìyánjiū
AT wánghóngzōng bōlíliàngānglúcháyīngyòngyúgāoxìngnénghùnníngtǔzhīgōngchéngxìngzhìyánjiū
_version_ 1718322071254073344