The suitability of continuous laminated veneer lumber production to some Canadian wood species
Laminated veneer lumber was made by gluing six layers of 1/4-inch veneer assembled with grain directions parallel and all the tight veneer surfaces outward. A specially modified phenol-formaldehyde plywood resin was used. Shear strength and wood failure of specimens tested dry, and after accelerated...
Main Author: | Afolayan, Ademola Adeniyi |
---|---|
Language: | English |
Published: |
2010
|
Online Access: | http://hdl.handle.net/2429/18832 |
Similar Items
-
THE EFFECTS OF WOOD SPECIES, LOAD DIRECTION, AND ADHESIVES ON BENDING PROPERTIES OF LAMINATED VENEER LUMBER
by: Bekir Cihad Bal,, et al.
Published: (2012-05-01) -
Surface roughness of thin wood veneers sliced from laminated green wood lumber
by: Guangyao Li, et al.
Published: (2018-01-01) -
Characteristics of lathe check and surface roughness of fast growing wood veneers and their performance on laminated veneer lumber
by: Rahayu-Sekartiing, Istie
Published: (2016) -
Fire Performance of Connections in Laminated Veneer Lumber
by: Chuo, Terence Chung Biau
Published: (2008) -
PROPERTIES OF LAMINATED VENEER LUMBER MANUFACTURED FROM HEAT TREATED VENEER
by: Hamiyet Sahin KOL, et al.
Published: (2016-06-01)