Production of Al2O3–SiC nano-composites by spark plasma sintering

In this paper, Al2O3–SiC composites were produced by SPS at temperatures of 1600 °C for 10 min under vacuum atmosphere. For preparing samples, Al2O3 with the second phase including of micro and nano-sized SiC powder were milled for 5 h. The milled powders were sintered in a SPS machine. After sinter...

Full description

Bibliographic Details
Main Authors: Mansour Razavi, Ali Reza Farajipour, Mohammad Zakeri, Mohammad Reza Rahimipour, Ali Reza Firouzbakht
Format: Article
Language:English
Published: Elsevier 2017-07-01
Series:Boletín de la Sociedad Española de Cerámica y Vidrio
Subjects:
SPS
XRD
Online Access:http://www.sciencedirect.com/science/article/pii/S0366317517300171