Effect of Postweld Heat Treatments on Type IV Creep Failure in the Intercritical Heat-Affected Zone of 10% Cr Martensitic Steel Welded with Haynes 282 Filler

This study investigated the effect of postweld heat treatment (PWHT) conditions on Type IV failure behavior of 10% Cr martensitic steel welds using Haynes 282 filler. The welded joints were subjected to PWHT at temperatures of 688, 738, and 788 °C for 4 and 8 h. Creep tests were carried out at 600 °...