Blistering and deuterium retention in Nb-doped W exposed to low-energy deuterium plasma
Tungsten and tungsten-niobium alloy with niobium concentration of 5 wt% were exposed to deuterium plasma at ~470 – 506 K, with flux of ~1.8 × 1021 D/m2/s, an ion energy of 100 eV and fluence of 1.3 × 1025 D/m2 – 5.2 × 1025 D/m2. Before exposure, the hardness and Young's modulus as well as latti...