High performance of solvothermally prepared VO2(B) as anode for aqueous rechargeable lithium batteries
The VO2 (B) was synthesized via a simple solvothermal route at 160oC in ethanol. The initial discharge capacity of VO2 (B) anode, in saturated aqueous solution of LiNO3, was 177 mAh g-1 at a current rate of 50 mA g-1. After 50 cycles capacity fade was 4%, but from 20th-50th cycle no capacit...