Microstructural Evolution and Strengthening Mechanism of SiC/Al Composites Fabricated by a Liquid-Pressing Process and Heat Treatment
Aluminum alloy (Al7075) composites reinforced with a high volume fraction of silicon carbide (SiC) were produced by a liquid-pressing process. The characterization of their microstructure showed that SiC particles corresponding to a volume fraction greater than 60% were uniformly distributed in the...