Spheroidization and Coarsening of Eutectic Si Particles in Al-Si-Based Alloys

The present study was carried out on three Al-Si cast alloys viz., 319, 356, and 413 alloys, solidified at 8°C/s. Samples from 319 and 413 alloys were solution heat-treated at 510°C, whereas samples from 356 alloy were solutionized at 550°C, for up to 1200 h. The results reveal that complete spheroi...