DEGRADATION OF 0.5Cr-0.5Mo-0.25V STEEL MICROSTRUCTURE DURING EXPLOITATION
Degradation of 0.5Mo-0.5Cr-0.25V material after long-term high-temperature service has been studied by means of microstructure and mechanical properties analysis. Samples were taken from the pipeline with steam leaking found after almost 200,000 h service at 565 °C. The microstructure and properties...