Laser deposition additive manufacturing of 17-4PH stainless steel on Ti-6Al-4V using V interlayer
For the first time, additive manufacturing was used to obtain a strong joint (bonding strength >200 MPa) between stainless steel and Ti-6Al-4V using a V interlayer. The V interlayer applied via solid-state joining prevented the formation of brittle intermetallic phases more effectively than a V i...