Microstructural and Electrical Properties of Sn-Modified BaTiO3 Lead-Free Ceramics by Two-Step Sintering Method

Ba(Ti0.92Sn0.08)O3 lead-free ceramics were prepared using a two-step sintering (TSS) technique. Varying the first sintering temperature T1 (1400 and 1500°C) and the dwell time t1 (0, 15, and 30 min), we obtained dense ceramics which were then soaked at a constant temperature of 1000°C (T2) for 6 h (...