Impact Strength of Austenitic and Ferritic-Austenitic Cr-Ni Stainless Cast Steel in -40 and +20°C Temperature

Studies described in this paper relate to common grades of cast corrosion resistant Cr-Ni steel with different matrix. The test materials were subjected to heat treatment, which consisted in the solution annealing at 1060°C followed by cooling in water. The conducted investigations, besides the micr...

Full description

Bibliographic Details
Main Authors: Kalandyk B., Zapała R., Boroń Ł., Solecka M.
Format: Article
Language:English
Published: Polish Academy of Sciences 2014-10-01
Series:Archives of Metallurgy and Materials
Subjects:
Online Access:http://www.degruyter.com/view/j/amm.2014.59.issue-3/amm-2014-0190/amm-2014-0190.xml?format=INT