Sintered Glass-Ceramics, Self-Glazed Materials and Foams from Metallurgical Waste Slag

The materials used for the synthesis of parent glass are 70 % wt. metallurgical slag and 30 % wt. industrial quartz sand. The initial batch is melted at and then quenched in water. The resulting glass frit is milled bellow 75 microns and pressed 1400 °C into “green” samples.In a next stage, they are...