Hot Deformation of the Mn-Ni-Cr Alloy During Compression

In this paper a constitutive equation was considered for the isothermal hot compression test of the Mn-Ni-Cr alloy. The hot compression test was performed in the strain rate range of 0.001-0.1 s-1 and deformation temperature was varied from 700 to 900 °C. A considerable reduction in flow stress was...

Full description

Bibliographic Details
Main Authors: M. Sadeghi, M. Hadi, O. Bayat, H. Karimi
Format: Article
Language:English
Published: Iran University of Science & Technology 2020-03-01
Series:Iranian Journal of Materials Science and Engineering
Subjects:
Online Access:http://ijmse.iust.ac.ir/article-1-1471-en.html