Significant improvement in Curie temperature and piezoelectric properties of BaTiO3 with minimum Pb addition
Dense Ba1-xPbxTiO3 (x = 0–0.20) samples (>90% TD) were fabricated through a solid-state reaction route involving wet ball milling for 24 h and calcination at 1150°C for 4 h, followed by sintering at 1300°C for 4 h. XRD results for all the samples revealed a tetragonal perovskite (P4mm) crystal st...