Grain growth in calibre rolled Mg–3Al–1Zn alloy and its effect on hardness

Calibre rolling of Mg–3Al–1Zn alloy at 300 °C led to development of fine grain size of 3 µm. Subsequent annealing, from 5 to 6000 minutes at 300–450 °C, revealed faster grain growth initially up to 60 minutes, which became sluggish on prolonged annealing. The time exponent for grain growth kinetics...