Effect of Carbon Addition and Mixture Method on the Microstructure and Mechanical Properties of Silicon Carbide

High dense (>99% density) SiC ceramics were produced with addition of C and B<sub>4</sub>C by spark plasma sintering method at 1950 °C under 50 MPa applied pressure for 5 min. To remove the oxygen from the SiC, it was essential to add C. Two different mixture method were used, dry mix...