Low temperature sintering of mechanically activated BaCO3-TiO2
In this article low temperature sintering of mechanically activated BaCO3-TiO2 system was studied. A stoichiometric mixture of BaCO3 and TiO2 powders was mechanically activated in a high-energy vibromill for 0, 30, 90 and 180 min, calcined at 800oC for 1 h and reaction sintered at 1100oC and 1200oC...